The 316L Austenitic Stainless Steel Pipe is a premium grade tubing with enhanced corrosion resistance, particularly against chloride pitting and crevice corrosion. Its low carbon content ensures resistance to intergranular corrosion, making it suitable for demanding applications in the marine, chemical, and food processing industries. Its austenitic structure provides excellent formability, weldability, and strength.
Invia la tua richiesta
Chatta adesso
introduzione al prodotto

The 316L Austenitic Stainless Steel Pipe is a highly regarded material in various industries.316L stainless steel is a molybdenum-bearing austenitic stainless steel, containing approximately 16-18% chromium, 10-14% nickel, and up to 2-3% molybdenum, along with a maximum carbon content of 0.03%. The addition of molybdenum significantly enhances its corrosion resistance, particularly against chloride ions.

Its austenitic microstructure, characterized by a face-centered cubic crystal lattice, contributes to its excellent ductility, toughness, and formability.

Corrosion Resistance: 316L stainless steel exhibits superior corrosion resistance in a wide range of environments, including those with high chloride concentrations, such as seawater and many chemicals. It is highly resistant to pitting and crevice corrosion, making it ideal for use in corrosive environments.

Intergranular Corrosion Resistance: The low carbon content of 316L stainless steel minimizes the risk of intergranular corrosion, particularly in welded joints. This feature allows it to maintain its corrosion resistance even after welding.

Formability and Weldability: The austenitic structure of 316L stainless steel makes it highly formable and easy to weld using various welding methods. It can be readily shaped into complex geometries and joined with other parts.

Strength and Toughness: Despite its excellent corrosion resistance, 316L stainless steel also possesses good strength and toughness, enabling it to withstand various loads and stresses.

Seamless Pipe 6MM - 1174MM or customized
Seamless Pipe 1mm - 80mm or customized
Seamless Pipe 12000mm or customized
2B, Pickling, Polished, Brushed, Sandblast, BA, EP

product-463-348product-348-347

Q1: What's your terms of payment?

A: 30%T/T as the upfront deposit, 70% before delivery, We will show you the photos and package before you pay the balance.

Q2: What's the terms of delivery?

Q3: What's the terms of packing?

Q4: What's your delivery time?

A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit. For production period, it usually takes about 15 days to 30 days after we received the deposit.

Q5: Could you produce according to the samples?

A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.

Etichetta sexy: 316l austenitic stainless steel pipe, China 316l austenitic stainless steel pipe manufacturers, suppliers, Tubo saldato in acciaio inossidabile A213 T22 T91, A213 T5 T9 T11 ERW Pipe, TUBING ASTM A213, ASTM A358 TP310 TP316 TUBO ACCIAIO EFW, JIS G3459 G3461 G3462 Tubo saldato in acciaio inossidabile, Pipe rotonde per ruota panoramica

Invia la tua richiesta

whatsapp

Telefono

Posta elettronica

Inchiesta